All samples were prepared from same perovskite precursor which was prepared with 1:3 molar ratio of lead acetate trihydrate and methylammonium iodide dissolved in dimethylformamide (Supplementary Note 5). For the samples with PMMA between the glass and perovskite layer, PMMA was spin-coated on the clean substrates at 3000 rpm for 30 s and annealed at 100 °C for 10 min. The perovskite precursor was spin-coated at 2000 rpm for 60 s on glass or glass/PMMA substrates, following by a 25 s dry air blowing, a 5 min room temperature drying and a 10 min 100 °C annealing. For the samples with PMMA on top of the perovskite layer, no further annealing was applied after the PMMA deposition.

Do you have any questions about this protocol?

Post your question to gather feedback from the community. We will also invite the authors of this article to respond.

post Post a Question
0 Q&A