2.1. High-Performance Concrete Mixture

RF Richard Fürst
EF Eliška Fürst
TV Tomáš Vlach
Jakub Řepka
MP Marek Pokorný
VM Vladimír Mózer
ask Ask a question
Favorite

The HPC mixture used for the preparation of experimental samples was prepared according to Table 1. This HPC mixture was developed at the Czech Technical University in Prague, Czech Republic. By following the prescribed procedure, this material can reach a compressive strength of about 140.5 MPa according to [36], a tensile strength of 15.4 MPa according to [37], and a modulus of elasticity value of about 49.5 GPa [4].

HPC component mixture of [4].