Preparation of direct metal laser sintered copings

SU Sujana Ullattuthodi
KC Kandathil Phillip Cherian
RA R. Anandkumar
MN M. Sreedevi Nambiar
request Request a Protocol
ask Ask a question
Favorite

Copings were made in the DMLS machine [EOSINT M270, EOS GmbH, Germany, Figure 7]. The ten working models were read by the scanner, using Cambridge software, by an experienced dental technician. Cobalt-chromium copings of 0.5 mm thickness, with a 50 μm of cement film thickness and short of their cervical margin by 0.5 mm, were designed.

Direct metal laser sintering machine (EOSINT M270, EOS GmbH, Germany)

DMLS technology fuses metal powder into a solid part by melting it locally using the focused laser beam and was builtup additively layer by layer, using layers of 20 μm thickness. A total of 10 DMLS copings were fabricated [Figure 8].

Direct metal laser sintered copings on the working models

Do you have any questions about this protocol?

Post your question to gather feedback from the community. We will also invite the authors of this article to respond.

0/150

tip Tips for asking effective questions

+ Description

Write a detailed description. Include all information that will help others answer your question including experimental processes, conditions, and relevant images.

post Post a Question
0 Q&A