The chemical composition of the RS was determined according to the chemical analysis methods reported by Teramoto et al. [24]. Specifically, holocellulose content was determined via weighting the NaClO2-delignified residue; cellulose content was determined via weighting the insoluble residue of holocellulose in the 17.5% NaOH aqueous solution; lignin content was determined via weighting the insoluble residue in 72% sulfuric acid aqueous solution. All experiments were carried out in triplicate.