2.7. Compressive Mechanical Properties of Hydrogels

XS Xi Song
CZ Chenhui Zhu
DF Daidi Fan
YM Yu Mi
XL Xian Li
RF Rong Zhan Fu
ZD Zhiguang Duan
YW Ya Wang
RF Rui Rui Feng
ask Ask a question
Favorite

The compression properties of the wet hydrogel (15 mm in diameter and 10 mm height) were tested using an INSTRON 5565 Materials Testing Machine (Instron, Norwood, MA, USA) at a loading rate of 10 mm/min. The compression strain of the wet HLCC hydrogel and the wet HLCS hydrogel were 60% and 80%, respectively.