An amount of 0.5 g of ZnO was dispersed with silica (90 wt%), and then the resultant suspension was sonicated for 5 min, stirred overnight in LiOH by centrifugation, and washed four times with ethanol/water mixture (19:1) to remove residual ionic compounds, and then dried in a vacuum oven at 333 K.