XRD mineral content examination utilized a D8 Discover X-ray diffractometer in accordance with the oil and gas industry standard (SY/T5463-2010). Shale samples were crushed to less than 300 mesh, combined with ethanol, mashed into a mortar, and then coated and put on slides for XRD testing.