The synthesized nanoparticles were dispersed in water, sonicated for 5 min, placed in dedicated cuvettes (DTS0012), and subjected to DLS analysis using a Nano ZS Zetasizer (Malvern Instruments, Malvern, UK). Measurements were performed at a spreading angle of 90° and a temperature of 25 °C; the reported values for average hydrodynamic diameter, polydispersity index, and Zeta potential are the average of five measurements.