The TH-NEG sample was positioned on a level testing surface within a glass jar to prevent premature activation and the formation of air bubbles. The evaluation of the firmness, cohesiveness, consistency, and viscosity of the sample was performed using a texture analyzer (TA. Plus, Stable Micro Systems, Surrey, UK) in a compression mode [10]. Force–time graphs were utilized to assess various texture profile attributes of TH-NEG.