Fabrication of PPFs-derived solid-state electrolytes (PPF-SSEs) powder

SC Shengmei Chen
YY Yiran Ying
LM Longtao Ma
DZ Daming Zhu
HH Haitao Huang
LS Li Song
CZ Chunyi Zhi
request Request a Protocol
ask Ask a question
Favorite

The PPF-SSEs are fabricated by ion diffusion. 0.5 g PPF nanosheets are dispersed in 50 mL 0.5 M Zn(OTf)2 trimethyl phosphate (TMP) solution under subatmospheric pressure condition and evaporates TMP solvent at 120 oC under vacuum condition for several times to get enough Zn2+ in PPF channels. After that, the PPF-SSEs are obtained by washing residual Zn(OTf)2 on the surface of PPFs with TMP and activated at 150 oC in vacuum for 12 h.

Do you have any questions about this protocol?

Post your question to gather feedback from the community. We will also invite the authors of this article to respond.

0/150

tip Tips for asking effective questions

+ Description

Write a detailed description. Include all information that will help others answer your question including experimental processes, conditions, and relevant images.

post Post a Question
0 Q&A