2.4. Swelling characterization of hydrogels

YW Y. Wang
YJ Y. Jia
HR H. Ren
CL C. Lao
WP W. Peng
BF B. Feng
JW J. Wang
ask Ask a question
Favorite

The as-prepared hydrogels were immersed in phosphate-buffered saline (PBS) until a swelling equilibrium was attained. The swelling ratio of the gels was calculated from the following equation:

where Ws is the mass of swollen hydrogel and Wd is the mass of dried hydrogel.