The membranes were obtained by casting DMSO solutions of SPP-TP-f polymers (2–3 wt.%) onto a flat glass plate and dried at 80°C overnight. The obtained membranes were immersed in 1 M HCl for 24 hrh and then washed with deionized water thoroughly.