PIM-EA-TB (Figure 1a) was prepared and characterised using a previously reported procedure [25].
(a) Chemical structure of Polymer of Intrinsic Microporosity derived from ethanoanthracene and Tröger’s base (PIM-EA-TB). (b) Electrospun fibrous mat of PIM-EA-TB.
Chloroform was purchased from VWR and used without purification. n-Propyl lactate was kindly provided by Corbion and used without purification. The physical properties of each solvent are shown in Table 1.
Physical properties of the solvents (a) obtained from MSDS and (b) measured.