Texture profile analysis (TPA) was carried out on the samples using a TA. TX Plus Texture Analyser (Stable Micro Systems Ltd., Surrey, UK). 1 cm3 gel samples were compressed using a 2 mm cylindrical probe according to the conditions described by Delgado and Bañón (2015), except a 0.01 N trigger force was used. Hardness (peak force during the double compression) was evaluated for the samples.