All procedures for the measurement of electrical conductivity were carried out in glove boxes filled with high-purity Ar (99.999%). To measure the electrical properties of 2D-LiZnSb and 3D-ZnSb, electrical contacts in the six-point probe configuration were made with silver epoxy. Then, Apiezon N grease was coated onto the sample surfaces to prevent oxidation of samples during measurements. For 2D-ZnSb, we adopted the stamp method, where the 2D-ZnSb was cleaved by 3M Scotch tape and the exfoliated crystal was pressed with 3M Scotch tape onto the patterned electrodes on a SiO2/Si wafer. The transferred sample was then pressed with a copper plate and firmly fixed.

Note: The content above has been extracted from a research article, so it may not display correctly.



Q&A
Please log in to submit your questions online.
Your question will be posted on the Bio-101 website. We will send your questions to the authors of this protocol and Bio-protocol community members who are experienced with this method. you will be informed using the email address associated with your Bio-protocol account.



We use cookies on this site to enhance your user experience. By using our website, you are agreeing to allow the storage of cookies on your computer.