Single crystals of FGT were prepared by chemical vapor transport (CVT) method with iodine as the transport agent. High-purity (99.99%) Fe, Ge, and Te were milled into powder form with a stoichiometric molar proportion of 3:1:2 (Fe:Ge:Te) in an agate mortar.