To improve surface adhesion of the printed structures to the substrate, we silanized the coverslips by activating the glass surface using plasma etching for 30 min and immersing them into 1 mM solution of 3-(trimethoxysilyl)propyl methacrylate in toluene afterward. Next, the coverslips were rinsed with isopropanol and blow-dried with a nitrogen gun.