Al foil (0.25 mm thick, annealed; 99.99%; Alfa Aesar) was used as the source of anode. Before using, the Al foil, which was used as the common Al anode, was polished with sand paper until the surface shined with metallic luster. For IL-treated Al anode (TAl), the common Al was impregnated in the IL electrolyte for more than 1 day. Then, the wet surface was cleaned before using for characterization and assembling any types of batteries.