All stress-strain curves were obtained from an HY-0580 tension machine (HENGYI Company). The cylindrical shaped tested samples (height, 15 mm; diameter, 4.72 mm) were first molded in plastic injection syringes, and the samples were then fixed on the jigs of the tension machine by two glass slices. The initial length (5 mm) was considered as the gap between the two edges of the glass slices. Unless otherwise noted, the tensile stress was measured at a constant speed of 200 mm/min. The data were recorded in real time by a connected computer.

Note: The content above has been extracted from a research article, so it may not display correctly.



Q&A
Please log in to submit your questions online.
Your question will be posted on the Bio-101 website. We will send your questions to the authors of this protocol and Bio-protocol community members who are experienced with this method. you will be informed using the email address associated with your Bio-protocol account.



We use cookies on this site to enhance your user experience. By using our website, you are agreeing to allow the storage of cookies on your computer.