To test the permeability of the HCS shell, HCS electrodes and ALD Al2O3/HCS electrodes were soaked in both battery electrolyte and saturated NaCl/H2O solution overnight. Electrodes were then taken out of the liquid. Electrodes soaked in the battery electrolyte were dried inside the glove box, and electrodes soaked in saturated NaCl solution were dried in an ambient environment.