2.4. Preparation of the PB@PDA@GQDs nanocomposites (PBPGs)

MW Meng Wang
BL Baolong Li
YD Yu Du
HB Huimin Bu
YT Yanyan Tang
QH Qingli Huang
ask Ask a question
Favorite

0.5 mg PBPs were dispersed in 1 mL deionized water by ultrasonication. Then, 2 mL (1 mg mL−1) GQDs were added to the above solution at 60 °C and oscillated for 6 h. Then, the resulting products were collected by the same method as that for the PBs.